Monash University
Browse

Fatigue cracking in aluminium alloy 7050-T7451 : quantitative fractographic methods and life prediction

thesis
posted on 2021-06-22, 00:52 authored by Simon Barter
<p>The author retains copyright of this thesis. It must only be used for personal non-commercial research, education and study. It must not be used for any other purposes and may not be transmitted or shared with others without prior permission. For further terms on this licence: </p> <a href="https://rightsstatements.org/page/InC-EDU/1.0/?language=en">https://rightsstatements.org/page/InC-EDU/1.0/?language=en</a><p></p> <p>Contact your local institution's library to make a resource sharing request for this thesis.</p>

History

Campus location

Australia

Year of Award

2007

Department, School or Centre

Mechanical and Aerospace Engineering

Course

Doctor of Philosophy

Degree Type

DOCTORATE

Faculty

Faculty of Engineering

File Name

Barter-33168027190863

Usage metrics

    Faculty of Engineering Theses

    Categories

    No categories selected

    Exports

    RefWorks
    BibTeX
    Ref. manager
    Endnote
    DataCite
    NLM
    DC